Green Basic Nickel Carbonate Powder, 45–48% Ni, for Battery-Material Production Evaluation
-
ColorLight greenPhysical formPowder
-
CAS No.12607-70-4Purity45%
-
AppearanceLight Green PowderApplicationBattery Materials, Catalysts, Electroplating Chemi
-
ClassificationCarbonateEINECS No.235-715-9
-
Grade StandardIndustrial GradeMolecular FormulaNiCO3*2Ni(OH)2*4H2O
-
Other NamesBasic Nickel Carbonate; Nickel Carbonate Basic; NiTypeNickel Carbonate
-
Product NameBasic Nickel CarbonateNickel Content45%-48%
-
DensityApprox. 3.5-4.0 g/cm³Water SolubilityInsoluble in Water
-
pH Value7.0-9.0Packing25kg PP Bag with PE Liner; 500kg/1000kg Jumbo Bag
-
HS Code2836999000Shelf Life24 Months
-
StorageStore in a Cool, Dry and Well-Ventilated PlaceSampleAvailiable
Battery-material selection begins with a defined component and an agreed analytical brief. This basic nickel carbonate is an industrial light green powder with stated nickel content of 45–48%. Battery-material production is an enquiry context for evaluating the powder.
Match the carbonate enquiry to the battery component
Identify the intended chemistry, process stage and constituent limits before requesting an evaluation sample. Ask which composition and particle measurements the project will use for acceptance. An industrial material designation does not establish battery-grade status or electrochemical performance.
Confirm basic carbonate identity with current documents
The stated formula is NiCO3*2Ni(OH)2*4H2O. Obtain compound-specific identity documentation that follows the actual sample, together with current elemental nickel analysis. The nickel-content range must remain separate from any claim about the purity of the whole compound.
Questions for a meaningful material comparison
What conditions were used for pH?
The reported material pH is 7.0–9.0. Request the preparation procedure and test concentration before comparing reports or deciding how the powder will be assessed.
How should the density be interpreted?
Density is stated as approximately 3.5–4.0 g/cm³. Confirm the measurement method and retain its approximate qualification; this value does not predict a finished battery result.
Agree the acceptance criteria before the actual-component trial and keep the results linked to the tested material. Catalyst or electroplating projects need separate process evidence, so specify the intended use when requesting technical and handling documents.